Creep Testing Unit

Creep Testing Unit

Categories: Lab Equipment


Creep Testing Unit Specification [1] Table unit for the investigation of the creep behaviour of different materials [2] Flat specimens made of lead and PE [3] Specimen cross-section 2x5mm, measured...

Product Code: ASLE075

  • ISO Certified
  • 24x7 Support
  • High Quality
  • After Sales Service
Product

About this product

Creep Testing Unit

Specification [1] Table unit for the investigation of the creep behaviour of different materials [2] Flat specimens made of lead and PE [3] Specimen cross-section 2x5mm, measured length 25mm [4] Tensile stress range 5...25N/mm² [5] Position measurement gauge 0...10mm, resolution 0.01mm [6] Experiments above or below room temperature possible with conditioning box Technical Data Specimen - material: lead, PE - cross-section: 2x5mm - measured length: 25mm Tensile stress range: 5...25N/mm² Position measurement - range: 0...10mm - resolution 0.01mm